| Austenitic stainless steel | Type 304; UNS S30400 | Moderate; generally below molybdenum-bearing grades | Concrete with limited chloride exposure, inland structures, or locations where chloride loading is controlled | Widely recognized alloy family; good general corrosion resistance and ductility | Not usually the first choice for severe marine splash zones or heavy deicing-salt exposure. Confirm the project’s chloride limits, cover, and service-life requirements. |
| Molybdenum-bearing austenitic stainless steel | Type 316; UNS S31600 | Higher than Type 304 in chloride-bearing environments | Coastal concrete, marine atmospheres, and structures exposed to road-salt spray or runoff | Molybdenum improves resistance to localized corrosion compared with Type 304 | Performance still depends on chloride concentration, concrete quality, cracking, cover, and detailing. Verify the exact product standard and certified chemistry. |
| Low-carbon molybdenum-bearing austenitic stainless steel | Type 316L; UNS S31603 | Similar general chloride-resistance category to Type 316 | Marine and deicing-salt exposure where a low-carbon 316-family specification is required | Low carbon content can reduce sensitization risk during welding compared with standard-carbon 316 | Low carbon does not by itself make the bar immune to chloride corrosion. Check whether welding is permitted and whether the selected rebar product is qualified for the intended fabrication. |
| Duplex stainless steel | 2205; commonly UNS S32205 or S31803, depending on specification | High; generally stronger chloride-corrosion resistance than 304 or 316-family grades | Severe marine exposure, splash and tidal zones, heavily salted bridge decks, and other high-chloride locations | Duplex microstructure combines austenitic and ferritic phases; commonly offers higher strength than standard austenitic grades as well as strong chloride resistance | Confirm the exact UNS grade, applicable rebar specification, design properties, fabrication requirements, and supply availability. Do not assume the two UNS designations are interchangeable without checking the purchase specification. |
| Lean duplex stainless steel | 2304; UNS S32304 | Generally above 304; typically below 2205 for demanding chloride service | Moderate-to-high chloride exposure where the project requires a duplex option and the exposure assessment supports it | Duplex structure and strength characteristics; contains less alloying than 2205 | Do not substitute for 2205 solely on the basis of the “duplex” label. Compare project-specific corrosion requirements, product qualification, and lifecycle cost. |